AWS ECuSi CopperAlloy Electrode ti a bo Electrodes T207 Arc Ejò Stick Stick Welding Rods

Apejuwe kukuru:

T207 (AWS ECuSi) jẹ elekiturodu alloy Ejò pẹlu mojuto idẹ silikoni ati ideri iṣuu soda hydrogen kekere.


Alaye ọja

ọja Tags

Ejò ati Ejò Alloy Welding Electrode

T207                                                     

GB/T ECuSi-B

Aws A5.6 ECuSi

 

Apejuwe: T207 ni a Ejò alloy elekiturodu pẹlu ohun alumọni idẹ mojuto ati kekere hydrogen soda ti a bo.Lo DCEP (daadaa elekiturodu lọwọlọwọ taara) pẹlu awọn ohun-ini ẹrọ ẹrọ nla.O ni ipata ti o dara si awọn acids inorganic miiran ju acid nitric, julọ Organic acids ati omi okun.

 

Ohun elo: O dara fun alurinmorin ti bàbà, ohun alumọni idẹ ati idẹ, surfacing alurinmorin ti linings ti kemikali pipelines ẹrọ, ati be be lo.

 

Apapọ kemikali ti irin weld (%):

Cu

Si

Mn

Pb

Al+Ni+Zn

92.0

2.5 ~ 4.0

≤3.0

≤0.02

≤0.50

 

 

Awọn ohun-ini ẹrọ ti irin weld:

试验项目

Ohun elo idanwo

抗拉强度

Agbara fifẹ

Mpa

延伸率

Ilọsiwaju

%

保证值

Ẹri

≥270

≥20

 

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

3.2

4.0

5.0

Alurinmorin Lọwọlọwọ

(A)

90 ~ 130

110 ~ 160

150 ~ 200

 

Akiyesi:

Àwọn ìṣọ́ra:

1. Awọn elekiturodu gbọdọ wa ni ndin ni nipa 300 ° C fun 1 to 2 wakati ṣaaju ki o to alurinmorin;

2. Ọrinrin, epo, oxides ati awọn impurities miiran lori dada ti weldment gbọdọ wa ni kuro ṣaaju ki o to alurinmorin.

3. Nigbati alurinmorin ohun alumọni idẹ tabi surfacing alurinmorin lori irin, ko si preheating wa ni ti beere.Iwọn otutu ti o ṣaju fun alurinmorin bàbà funfun jẹ nipa 450 ° C, ati iwọn otutu ti o ṣaju fun idẹ alurinmorin jẹ nipa 300 ° C;

4. Kukuru-aaki alurinmorin yẹ ki o wa lo nigba alurinmorin.Lakoko alurinmorin olona-Layer, slag laarin awọn fẹlẹfẹlẹ gbọdọ jẹ

patapata kuro;lẹhin alurinmorin, lu awọn weld pẹlu kan alapin ori ju lati liti awọn oka, imukuro wahala, ki o si mu awọn agbara ati ṣiṣu ti awọn weld.