ENiFe-CI Nickel Alloy Welding Waya, FN 55 Nickel Tig Wire Ferro-nickel Solid Waya

Apejuwe kukuru:

Ferro-nickel ri to waya ti a lo fun alurinmorin irin simẹnti ati ductile iron.


Alaye ọja

ọja Tags

Nickel AlloyWelding Waya Tig WayaENiFe-CI

Awọn ajohunše
EN ISO 1071 - SC NiFe-1
Aws A5.15 – E NiFe-CI

 

Awọn ẹya ara ẹrọ ati Awọn ohun elo

Ferro-nickelokun waya ti o lagbara ti a lo fun irin simẹnti alurinmorin ati irin ductile.

Dara fun awọn isẹpo ti o yatọ laarin irin simẹnti, irin kekere, alloy kekere ati awọn irin alagbara.

Iṣeduro fun alurinmorin imi-ọjọ giga, phosphorous tabi lubricant-ti doti simẹnti.

Ti a lo fun ọpọlọpọ awọn atunṣe ati awọn ohun elo iṣelọpọ, pẹlu awọn ọpa atunkọ, awọn kẹkẹ, awọn isẹpo pataki laarin irin ati irin simẹnti ati be be lo.

Awọn ohun elo Mimọ Aṣoju

Irin simẹnti grẹy, malleable, nodular*
* Apejuwe, kii ṣe atokọ pipe

 

Iṣọkan Kemikali%

C%

Mn%

Si%

P%

S%

   

o pọju

o pọju

o pọju

o pọju

o pọju

   

2.00

0.80

0.20

0.03

0.03

   

   

Fe%

Ni%

Ku%

Al%

   

rem.

54.00

o pọju

o pọju

   

56.00

2.50

1.00

   

 

Darí Properties
Agbara fifẹ 400 – 579 MPa  
Agbara Ikore -  
Ilọsiwaju -  
Agbara Ipa -  

Awọn ohun-ini ẹrọ jẹ isunmọ ati pe o le yatọ si da lori ooru, gaasi idabobo, awọn aye alurinmorin ati awọn ifosiwewe miiran.

 

Awọn eefin idabobo

EN ISO 14175 - TIG: I1 (Argon)

 

Alurinmorin Awọn ipo

EN ISO 6947 - PA, PB, PC, PD, PE, PF

 

Data apoti

Iwọn opin

Gigun

Iwọn

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

Layabiliti: Lakoko ti gbogbo awọn igbiyanju ironu ti ṣe lati rii daju deede alaye ti o wa ninu, alaye yii jẹ koko ọrọ si iyipada laisi akiyesi ati pe o le gba nikan bi o dara fun itọsọna gbogbogbo.

 