ERNiFeCr-1 nickel Alloy Welding Waya, Nickel Tig Waya Filler Metal

Apejuwe kukuru:

Alloy 825 (ERNiFeCr-1) jẹ okun waya nickel-iron-chromium ṣiṣe eyi ni yiyan ti o dara fun ọpọlọpọ awọn ohun elo ti o nira.


Alaye ọja

ọja Tags

Nickel AlloyWelding WayaTig WayaERNiFeCr-1

Awọn ajohunše
EN ISO 18274 – Ni 8065 – NiFe30Cr21Mo3
Aws A5.14 - ER NiFeCr-1

 

Awọn ẹya ara ẹrọ ati Awọn ohun elo

Alloy 825 jẹ anickel-irin-chromium waya ṣiṣe eyi ni yiyan ti o dara fun ọpọlọpọ awọn ohun elo ti o nira.

Waya yii n pese awọn ipele giga ti ipata ipata si mejeeji ni iwọntunwọnsi oxidising ati idinku awọn agbegbe.

Pipe fun ibori agbekọja nibiti o ti nilo akojọpọ kemikali ti o jọra.

O tayọ weldability pẹlu kikun austenitic weld irin pẹlu ga resistance lodi si wahala ipata wo inu media ti o ni awọn kiloraidi ions.

Ti a lo ni igbagbogbo ni awọn ile-iṣẹ iṣelọpọ kemikali, petrochemical, iṣelọpọ iwe ati iran agbara ati bẹbẹ lọ.

 

Awọn ohun elo Mimọ Aṣoju

G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, ALLOY 825 N25N1, UNOS 825.8. 4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465 , 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586*
* Apejuwe, kii ṣe atokọ pipe

 

Iṣọkan Kemikali%

C%

Mn%

Fe%

P%

S%

Si%

 

o pọju

0.70

22.00

o pọju

o pọju

o pọju

 

0.05

0.90

min

0.020

0.004

0.50

 

 

Ku%

Ni%

Al%

Ti%

Kr%

Mo%

 

2.30

43.00

o pọju

1.00

22.00

3.00

 

3.00

46.00

0.20

1.20

23.50

3.50

 

 

Darí Properties
Agbara fifẹ ≥550 MPa  
Agbara Ikore -  
Ilọsiwaju -  
Agbara Ipa -  

Awọn ohun-ini ẹrọ jẹ isunmọ ati pe o le yatọ si da lori ooru, gaasi idabobo, awọn aye alurinmorin ati awọn ifosiwewe miiran.

 

Awọn eefin idabobo

EN ISO 14175 - TIG: I1 (Argon)

 

Alurinmorin Awọn ipo

EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Data apoti
Iwọn opin Gigun Iwọn  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

 