E316HT1-1 Irin alagbara, irin ṣiṣan cored waya

Apejuwe kukuru:

O ni iṣẹ ṣiṣe alurinmorin ti o dara julọ gẹgẹbi arc iduroṣinṣin, spatter ti o dinku, yiyọ slag ti o dara, ifunni okun waya iduroṣinṣin, ati apẹrẹ ẹlẹwa


Alaye ọja

ọja Tags

E316HT1-1 Irin alagbara, irin ṣiṣan cored waya

ọja Apejuwe
Ni ibamu pẹlu bošewa: GB/T17853 E316T1-1
Aws A5.22 E316HT1-1

Awọn ẹya ara ẹrọ ati awọn lilo
1. Nitori ti o ni awọn kan awọn iye ti erogba, o jẹ o dara fun alurinmorin ga otutu sooro alagbara, irin ẹrọ;
2. O ni iṣẹ ilana alurinmorin ti o dara julọ gẹgẹbi arc iduroṣinṣin, kekere spatter, yiyọ slag ti o dara, ifunni okun waya iduroṣinṣin, ati apẹrẹ lẹwa;
3. Nitori akoonu ti o ga julọ ti Mo, ipata ipata lagbara;
4. Dara fun 18% Cr-12% Ni-2% Mo alurinmorin ni petrochemical, titẹ ọkọ, egbogi ati ounje ẹrọ, ajile ati awọn miiran ise.

Akopọ kemikali (wt%)

Alloy wt% C Mn Ati Cr In Mo P S Pẹlu
GB/T 0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.50
AWS 0.04-0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.75
Apeere iye 0.50 1.45 0.50 18.05 12.00 2.35 0.020 0.005 0.05

 
Darí ihuwasi

Darí ihuwasi Agbara ikore MPa Agbara fifẹ MPa Ilọsiwaju% Iye ipa J/℃
GB/T - 520 30 -
AWS - 520 30 -
Apeere iye - 560 35 -

 
Ibiti a ṣe iṣeduro lọwọlọwọ: (DC+)

Iwọn okun waya alurinmorin (mm) 1.2 1.6
Foliteji (V) 22-36 26-38
Lọwọlọwọ (A) 120-260 200-300
Gbigbe gbigbe (mm) 15-20 18-25
Ṣiṣan gaasi (l/min) 15-25 15-25

 
Awọn iṣọra alurinmorin
1. Lo CO2 gaasi aabo pẹlu mimọ ti ≥99.98% ati ṣiṣan gaasi ti 20-25L / min.
2. Inter-ikanni otutu: 16 ~ 100 ℃.
3. Nigbati alurinmorin, o jẹ pataki lati dabobo lati afẹfẹ lati se alurinmorin abawọn lati tuka ti awọn shielding gaasi.Epo, omi, ati bẹbẹ lọ ni ibi alurinmorin gbọdọ yọkuro.
4. Lo okun waya alurinmorin ni kete bi o ti ṣee lẹhin ṣiṣi package naa.Ti ko ba lo soke, gbe awọn igbese ẹri-ọrinrin.

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣiṣẹ ni iṣelọpọ awọn amọna alurinmorin,alurinmorin ọpá, ati alurinmorin consumables fun diẹ ẹ sii ju 20 ọdun.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.