Ìsọ̀rí AWS: AWS 5.9
ÀPÈJÚWE:
Wáyà ìsopọ̀mọ́ra irin alagbara ní agbára ìbòrí gíga, iṣẹ́ ìmọ̀-ẹ̀rọ ìsopọ̀mọ́ra tó dára ní gbogbo ipò ìsopọ̀mọ́ra. Wọ́n wọ́pọ̀ ní ilé-iṣẹ́: ìṣètò ilé, ọkọ̀, ìmọ̀-ẹ̀rọ afárá, ẹ̀rọ iwakusa, ọkọ̀ ojú irin, páìpù epo, ẹ̀rọ tí ń gbé ìfúnpá gaasi, ẹ̀rọ agbára, àti bẹ́ẹ̀ bẹ́ẹ̀ lọ.
Nọ́mbà Àwòṣe àti Ìwọ̀n:
1. Ipese ile-iṣẹ iṣẹ OEM.
2. Àwòṣe: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi àti bẹ́ẹ̀ bẹ́ẹ̀ lọ.
3. Ìwọ̀n wáyà MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Ìwọ̀n wáyà TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
ÌFÍHÀN:
A n pese oniruuru waya irin alagbara, pẹlu okun waya Mig solid welding, okun waya Tig rod welding ati okun waya submerged-arc welding, gbogbo wọn ni didara giga ati pe a n ta wọn kaakiri agbaye.
Yàtọ̀ sí 308 àti 309, a tún ń fúnni ní 304, 321, 347, 316L, 310, 2209, àti 201. Bákan náà pẹ̀lú àwọn ìlànà pàtàkì bíi 318L, 904L, 2594, NiCrMo-3, Ni1.
ÀKÓJỌ:
Iṣakojọpọ waya alurinmorin Mig (spool ati drum pack)
Ìwọ̀n ...
Àpò: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/spool, 200 kg/spool
Iṣakojọpọ waya alumọni Tig rod (ọpọn ṣiṣu)
Ìwọ̀n ...
Àpò: 5 kg/àpò
Wáìlì ìrọ̀lẹ̀ aaki tí a rì sínú omi
Ìwọ̀n ...
Àpò: 20kg/àpò, 25 kg/àpò
A kaabo apoti didoju ati OEM!
ÀWỌN ÌṢẸ̀LẸ̀ KẸ́MÍKÀ TI WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ:
| Nọmba awoṣe | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 |
|
|
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Nọmba awoṣe | Agbára ìfàsẹ́yìn Rm(Mpa) | Agbara ikore Rel tabi Rp0.2 (Mpa) | Gbigbọn (%) | Nọmba awoṣe | Agbára ìfàsẹ́yìn Rm(Mpa) | Agbara ikore Rel tabi Rp0.2 (Mpa) | Gbigbọn (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| Tiwqn waya irin alagbara TIG ati MIG ti a ṣe pẹlu irin alagbara TIG ati MIG | ||||||||||
| YB5092-2005 | AWS | Àkójọpọ̀ Kẹ́míkà % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo |
| ||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 |
|
|
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 |
|
|
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 |
|
|
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 |
|
|
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 |
|
|
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 |
|
|
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 |
|
|
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 |
|
|
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 |
|
|
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 |
|
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 |
|
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 |
|
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 |
|
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 |
|
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 |
|
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 |
| Ti9xC-1.0 |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 |
| Nb1xC-1.0 |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 |
|
|
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 |
|
|
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 |
|
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 |
| Cu;3 Nb;0.28 |
| H08Cr26Ni5Mo2 | ER453s | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 |
|
| H08Cr21Ni10Mn6 |
| 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 |
|
|
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |