AWS D507 Hardfacing Welding Electrodes Wọ Awọn ọpa Alurinmorin Resistant fun Arc Welding

Apejuwe kukuru:

Eyi jẹ elekiturodu alurinmorin wapọ fun alurinmorin yiya ti irin erogba tabi awọn ọpa irin alloy ati awọn falifu pẹlu iwọn otutu iṣẹ ni isalẹ 450 ° C.


Alaye ọja

ọja Tags

LO:

Eyi jẹ elekiturodu alurinmorin wapọ fun alurinmorin yiya ti irin erogba tabi awọn ọpa irin alloy ati awọn falifu pẹlu iwọn otutu iṣẹ ni isalẹ 450 ° C.

IṢẸ́ KẸ́MÍKÌ IRÍN OLÓÒ (%):

C

Cr

S

P

Miiran eroja ti lapapọ

iye onigbọwọ

≤0.15

10.00 ~ 16.00

≤0.030

≤0.040

≤2.50

Apeere iye

0.13

13.34

0.006

0.022

-

LÁRÌLẸ̀ LÉYÉ SÍRẸ̀:

(Itutu afẹfẹ lẹhin alurinmorin) HRC ≥ 40

Itọkasi lọwọlọwọ (DC +):

Iwọn elekitirodu (mm)

φ3.2

φ4.0

φ5.0

Alurinmorin lọwọlọwọ (A)

80 ~ 120

120 ~ 160

160 ~ 200

ÀWỌN ÌṢỌ́RA:

⒈ elekiturodu alurinmorin lati jẹ 300 ~ 350 ℃ yan 1h.

⒉ iṣaju alurinmorin iṣẹ-ṣiṣe lati wa ni preheated si 300 ℃ loke, lẹhin alurinmorin oriṣiriṣi itọju ooru le gba líle ti o yẹ.

OPA WELDING AWS E6010:

AWS E6010 ni a irú ti cellulose-Na iru alurinmorin amọna, pataki fun DC.O gba imọ-ẹrọ ajeji ti ilọsiwaju, o ni ARC ti o jinlẹ, awọn slags diẹ, iyọkuro irọrun, alurinmorin giga daradara, awọn ohun-ini iṣẹ ṣiṣe ẹlẹwa.O le ṣee lo fun alurinmorin fun gbogbo ipo, inaro si oke ati isalẹ ipo alurinmorin ati be be lo o le de ọdọ awọn ipa ti ọkan ẹgbẹ alurinmorin ni ẹgbẹ mejeeji Ibiyi.

Ohun elo:

Awọn ọpa alurinmorin AWS E6010 ni akọkọ fun alurinmorin paipu erogba tabi ohun elo kanna, weld atilẹyin / kikun weld / ohun ikunra fun eto irin isalẹ.

Iṣapọ Kemikali (%)

Awọn ohun-ini ẹrọ ti irin ti o GBE:

Nkan Idanwo Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Iye idaniloju ≥460 ≥340 ≥16 ≥47
Abajade gbogbogbo 485 380 28.5 86

Itọkasi lọwọlọwọ (DC):

Iwọn opin φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

AKIYESI:

1. O rọrun lati fi han si ọrinrin, jọwọ tọju rẹ ni ipo gbigbẹ.

2. O nilo alapapo nigbati package fi opin si tabi ọrinrin ti o gba, iwọn otutu alapapo yẹ ki o wa laarin 70C si 80C, akoko alapapo yẹ ki o jẹ lati 0,5 si 1 wakati.

3. Nigba lilo 5.0mm alurinmorin amọna, o dara lati lo ga-titari, kekere-lọwọlọwọ, ni ibere lati mu alurinmorin iṣẹ.

C Mn Si S P
<0.2 0.3-0.6 <0.2 <0.035 <0.04