Apejuwe kukuru:

AF2209-16 (AWS E2209-16) jẹ elekiturodu irin alagbara irin oloke meji ti o ni kekere nitrogen ti o ni kekere pẹlu titanium-calcium bo.


Alaye ọja

ọja Tags

Irin AlurinmorinElectrode

AF2209-16                               

GB/T E2209-16

Aws A5.4 E2209-16

Apejuwe: AF2209-16 jẹ elekiturodu irin alagbara irin olopo meji ti o ni kekere carbon nitrogen pẹlu titanium-calcium ti a bo.O le ṣee lo fun awọn mejeeji AC ati DC pẹlu iṣẹ ṣiṣe to dara julọ.Nitoripe o ni molybdenum ati nitrogen, ati akoonu erogba jẹ kekere pupọ, irin ti a fi silẹ ni o ni idena kiraki ti o dara ati idena ipata, ni pataki idena ipata wahala.

Ohun elo: O ti wa ni o kun lo fun alurinmorin iru kanna ti olekenka-kekere erogba alagbara, irin ohun elo ni Epo ilẹ ati eefun ti ise.Iru bii alurinmorin ti 022Cr22Ni5Mo3N duplex alagbara, irin.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Ilọsiwaju

%

Ẹri

≥690

≥20

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.5

3.2

4.0

5.0

Alurinmorin Lọwọlọwọ

(A)

50 ~70

80 ~ 110

130 ~ 150

160 ~ 200

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni ayika 250 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O ṣe pataki lati nu ipata, iwọn epo, omi, ati awọn impurities lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.

 

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣiṣẹ ni iṣelọpọ ti iṣelọpọ.alurinmorin elekiturodus, alurinmorin ọpá, atialurinmorin consumablesfun diẹ ẹ sii ju 20 ọdun.

Awọn ọja akọkọ wa pẹlu irin alagbaraalurinmorin elekiturodus, erogba irin alurinmorin elekitirodu, kekere alloy alurinmorin elekitirodu, surfacing alurinmorin elekitirodu, nickel & cobalt alloy alurinmorin elekitirodu, ìwọnba irin & kekere alloy alurinmorin onirin, irin alagbara, irin alurinmorin onirin, gaasi-idabobo flux cored wires, aluminiomu alurinmorin onirin, submerged arc alurinmorin .wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 