AWS E2594-16 Electrode alurinmorin, Awọn ọpá alurinmorin, Awọn ohun elo alurinmorin

Apejuwe kukuru:

AF2594-16 (AWS E2594-16) jẹ elekiturodu irin alagbara irin oloke meji ti o ni kekere nitrogen ti o ni kekere pẹlu titanium-calcium bo.


Alaye ọja

ọja Tags

Irin AlurinmorinElectrode

AF2594-16

Aws A5.4 E2594-16

Apejuwe: AF2594-16 jẹ elekiturodu irin alagbara irin olopo meji ti o ni kekere carbon nitrogen pẹlu titanium-calcium ti a bo.O le ṣee lo fun awọn mejeeji AC ati DC.PRE (pitting resistance deede iye tabi itọka pitting) ≥ 40, irin ti a fi silẹ ni o ni idaabobo igbona ti o dara.Nitori akoonu erogba kekere ati iye kan ti molybdenum ati nitrogen, irin ti a fi silẹ ni o ni resistance to dara si ipata pitting ati idaamu ipata wahala.

Ohun elo: O ti wa ni o kun lo fun alurinmorin iru kanna ti duplex alagbara, irin ni ti ilu okeere epo, adayeba gaasi ati petrochemical ise, gẹgẹ bi awọn 00Cr25Ni7Mo4N, ati be be lo.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤1.00

24.0 ~ 27.0

8.0 ~ 10.5

3.5 ~ 4.5

0.20 ~ 0.30

≤0.75

≤0.030

≤0.040

 

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Ilọsiwaju

%

Ẹri

≥760

≥15

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.5

3.2

4.0

5.0

Alurinmorin Lọwọlọwọ

(A)

50 ~80

80 ~ 120

120 ~ 150

150 ~ 200

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni ayika 250 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O ṣe pataki lati nu ipata, iwọn epo, omi, ati awọn impurities lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.

 

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣiṣẹ ni iṣelọpọ ti iṣelọpọ.alurinmorin elekiturodus, alurinmorin ọpá, atialurinmorin consumablesfun diẹ ẹ sii ju 20 ọdun.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 