AWS E9015-G Low Alloy Steel Welding Rod Kekere hydrogen Welding Electrodes J607CrNiMo

Apejuwe kukuru:

J607CrNiMo (AWS E9015-G) jẹ elekiturodu irin alloy kekere ti o ni ideri iṣuu soda hydrogen kekere.


Alaye ọja

ọja Tags

Low Alloy Irin Welding Electrode

J607CrNiMo                                       

GB/T E6015-G

Aws E9015-G

 

Apejuwe: J607CrNiMo jẹ elekiturodu irin alloy kekere kan pẹlu ideri iṣuu soda hydrogen kekere.Lo DCEP (taara ti isiyi elekiturodu rere), ati ki o le ti wa ni welded ni gbogbo awọn ipo pẹlu kukuru aaki isẹ.Ọpa alurinmorin ni ijinle ilaluja nla, spatter kere ati iṣẹ ṣiṣe to dara.Idogo irin ni o ni ti o dara ṣiṣu, kekere otutu toughness ati kiraki resistance.

Ohun elo: O ti wa ni lilo fun awọn alurinmorin ti omi ipese pipes ni isalẹ 350 °C ni agbara ibudo ati titẹ ọkọ irin ti o baamu agbara onipò.O ni ibaramu to dara pẹlu irin WB36CN1 (HD15Ni1MnMoNbCu) irin, ati pe o tun dara fun alurinmorin WB3 (15NiCuMoNb5) irin.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Cr

Ni

Mo

S

P

≤0.10

1.00 ~ 1,60

≤0.50

0.14 ~ 0.35

0.60 ~ 1.20

0.15 ~ 0.50

≤0.015

≤0.015

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Iye ipa (J)

-30 ℃

Ẹri

620 ~ 720

≥500

≥20

≥47

 

Akoonu hydrogen tan kaakiri ti irin ti a fi silẹ: ≤5.0mL/100g (Makiuri tabi ọna kiromatogirafi gaasi)

Ayewo X-ray: Mo ite

 

Iṣeduro lọwọlọwọ:

(mm)

Opa opin

3.2

4.0

5.0

(A)

Alurinmorin Lọwọlọwọ

100 ~ 140

140 ~ 18

190 ~ 230

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni ayika 350 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O ṣe pataki lati nu ipata, iwọn epo, omi, ati awọn impurities lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.