AWS ER308LSi Irin Alagbara Irin Alurinmorin Waya MIG ati TIG Welding Rods Filler Rods

Apejuwe kukuru:

Irin alagbara, irin alurinmorin waya ni o ni ga cladding ṣiṣe, ti o dara alurinmorin išẹ ni gbogbo-ipo alurinmorin.Wọn ti wa ni o gbajumo ni lilo ninu ile ise: ile awọn ẹya, ọkọ, Afara ina-, iwakusa ẹrọ, Reluwe, epo paipu, gaasi ti nso ẹrọ, agbara ẹrọ, ati be be lo.


Alaye ọja

ọja Tags

Isọri AWS:AWS 5.9

Apejuwe:

Irin alagbara, irin alurinmorin waya ni o ni ga cladding ṣiṣe, ti o dara alurinmorin išẹ ni gbogbo-ipo alurinmorin.Wọn ti wa ni o gbajumo ni lilo ninu ile ise: ile be, ọkọ, Afara ina-, iwakusa ẹrọ, Reluwe, epo paipu, gaasi ti nso ẹrọ, agbara ẹrọ, ati be be lo.

Awoṣe RARA.& Iwon:

1. Ipese ile-iṣẹ OEM iṣẹ.

2. Awoṣe: ER308 ER308L ER308Lsi ER309 ER309L ER316 ER316L ER316LSi ati be be lo.

3. MIG waya iwọn: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4.TIG waya iwọn: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.

ÌBÁLẸ̀:

A pese awọn oriṣiriṣi iru okun waya alurinmorin irin alagbara, pẹlu Mig ri okun waya alurinmorin, Tig rod welding wire and submerged-arc welding wire, gbogbo awọn ti ga didara ati ti wa ni tita agbaye.

Ayafi fun 308 ati 309, a tun funni ni 304, 321, 347, 316L, 310, 2209, ati 201. Bii awọn alaye pataki bi 318L, 904L, 2594, NiCrMo-3, Ni1.

Iṣakojọpọ:

Iṣakojọpọ waya alurinmorin Mig (spool ati idii ilu)

Opin: 0.8 - 2.0mm

Package: 1 kg / spool, 5 kg / spool, 15 kg / spool, 20 kg / spool, 100 kg / ilu, 200 kg / ilu

Iṣakojọpọ waya alurinmorin Tig opa (tube ṣiṣu)

Opin: 1.0 - 5.0mm

Package: 5 kg / idii

Submerged aaki alurinmorin waya

Opin: 2.5 - 5.0mm

Apo: 20kg/pack, 25 kg/pack

Apoti aiduro ati OEM ṣe itẹwọgba!

Awọn nkan kẹmika TI WÁ AWỌRỌ IRIN ALILÉ

Awoṣe No.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

Awọn ohun-ini ẹrọ ti WÁNṢẸ:

Awoṣe No.

Agbara fifẹ Rm(Mpa)

Agbara ikore Rel tabi Rp0.2(Mpa)

Ilọsiwaju

(%)

Awoṣe No.

Agbara fifẹ Rm(Mpa)

Agbara ikore Rel tabi Rp0.2(Mpa)

Ilọsiwaju

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

TIG ati MIG alagbara, irin alurinmorin waya tiwqn

YB5092-2005

AWS

Iṣọkan Kemikali%

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Ku 1,80

H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Kú;3 Nb;0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣe alabapin ninu iṣelọpọ awọn amọna alurinmorin, awọn ọpa alurinmorin, ati awọn ohun elo alurinmorin fun diẹ sii ju ọdun 20 lọ.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣe alabapin ninu iṣelọpọ awọn amọna alurinmorin, awọn ọpa alurinmorin, ati awọn ohun elo alurinmorin fun diẹ sii ju ọdun 20 lọ.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.


  • Ti tẹlẹ:
  • Itele: