AWS ER5183 Aluminiomu Welding Waya Aluminiomu MIG Awọn ọpa alurinmorin ati Tig Waya

Apejuwe kukuru:

ER5183 jẹ o dara fun MIG alurinmorin aluminiomu magnẹsia alloy ti o ga agbara fifẹ wa ni ti beere ati ti o ba ti mimọ irin ni 5083 tabi 5654 agbara fifẹ yoo jẹ Elo ti o ga.O ti wa ni o gbajumo ni lilo fun alurinmorin aluminiomu magnẹsia alloy ẹya ti awọn ọkọ, ti ilu okeere iru ẹrọ, locomotives & carriages, motor awọn ọkọ ti, awọn apoti, cryogenic èlò ati be be lo.


Alaye ọja

ọja Tags

ER5183 jẹ o dara fun MIG alurinmorin aluminiomu magnẹsia alloy ti o ga agbara fifẹ wa ni ti beere ati ti o ba ti mimọ irin ni 5083 tabi 5654 agbara fifẹ yoo jẹ Elo ti o ga.O ti wa ni o gbajumo ni lilo fun alurinmorin aluminiomu magnẹsia alloy ẹya ti awọn ọkọ, ti ilu okeere iru ẹrọ, locomotives & carriages, motor awọn ọkọ ti, awọn apoti, cryogenic èlò ati be be lo.Awọn oniwe-weld irin ni o ni ti o dara resistance to brine ipata.

Ipo alurinmorin: F, HF, V

Iru lọwọlọwọ: DCEP

AKIYESI:

Mimu package ti okun waya ni ipo ti o dara ṣaaju alurinmorin.

Mejeeji awọn ipele ti o yẹ ki o ṣe welded ti weldment ati okun waya gbọdọ wa ni mimọ kuro awọn aimọ ti idoti epo, bo oxide, ọrinrin ati bẹbẹ lọ.

Lati gba irisi ti o dara ti weld o jẹ dandan lati ṣaju irin ipilẹ si 100 ℃-200 ℃ ṣaaju alurinmorin ti sisanra rẹ ba jẹ 10mm tabi diẹ sii.

O dara lati fi subplate kan labẹ agbegbe weld lati tan irin yo o lati rii daju pe ilaluja weldment naa ni pipe.

Gẹgẹbi ipo alurinmorin ati sisanra ti irin ipilẹ ti o yatọ gaasi apata yẹ ki o yan, bii 100% Ar, 75% Ar + 25% He, 50% Ar + 50% He, bbl

Awọn ipo alurinmorin ti a mẹnuba loke fun itọkasi nikan ati pe o dara lati ṣe afijẹẹri ilana alurinmorin ni ibamu si iṣẹ akanṣe ṣaaju ki o to fi sii sinu alurinmorin deede.

ER5183 ILU KẸKAMI TI IRIN IGBESI (%):

SI FE CU MN MG CR ZN TI AI BE
Standard ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Iwontunwonsi ≤0.0003
Aṣoju 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Iwontunwonsi 0.0001

Awọn ohun-ini ẹrọ ti IRIN Idogo (AW):

AGBARA TINSILE RM (MPA) AGBARA YIELD (MPA) IGBỌN A4 (%)
Aṣoju 280 150 18

Awọn iwọn & Niyanju Lọwọlọwọ fun MIG (DC+):

DIAMETER WIRE WELDING (MM) 1.2 1.6 2.0
Alurinmorin Lọwọlọwọ (A) 180-300 200-400 240-450
Foliteji Alurinmorin (V) 18-28 20-20 22-34

Awọn iwọn & Iṣeduro Iṣeduro fun TIG (DCng):

DIAMETER WIRE WELDING (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Alurinmorin Lọwọlọwọ (A) 150-250 200-320 220-400

 

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣe alabapin ninu iṣelọpọ awọn amọna alurinmorin, awọn ọpa alurinmorin, ati awọn ohun elo alurinmorin fun diẹ sii ju ọdun 20 lọ.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 