J501Fe18 (AWS E7024) jẹ ẹya irin powder titanium-Iru ga-ṣiṣe erogba irin elekiturodu.


Alaye ọja

ọja Tags

Erogba Irin AlurinmorinElectrode

J501Fe18                                                

GB/T E5024

Aws A5.1 E7024

Apejuwe: J501Fe18 jẹ ẹya irin lulú titanium-Iru ga-ṣiṣe erogba, irin elekiturodu.Iṣe ṣiṣe ifisilẹ wa ni ayika 180%, eyiti o dara fun alurinmorin alapin ati alurinmorin fillet alapin.

Ohun elo: O ti wa ni lilo fun alurinmorin ti kekere erogba, irin, gbogboogbo agbara hull igbekale irin ClassA, Kilasi B ati ki o ga agbara hull igbekale irin AH32, AH36.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

S

P

≤0.12

≤1.25

≤0.60

≤0.035

≤0.035

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Iye ipa (J)

(0℃)

Ẹri

≥490

≥400

≥23

≥47

X-ray ayewo: II ite

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

3.2

4.0

5.0

5.6

6.0

Alurinmorin lọwọlọwọ

(A)

130 ~ 170

180 ~ 230

250 ~ 340

280 ~ 400

300 ~ 430

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣiṣẹ ni iṣelọpọ ti iṣelọpọ.alurinmorin elekiturodus, awọn ọpa alurinmorin, ati awọn ohun elo alurinmorin fun diẹ sii ju 20 ọdun lọ.

Awọn ọja akọkọ wa pẹlu irin alagbaraalurinmorin elekiturodus, erogba irin alurinmorin elekitirodu, kekere alloy alurinmorin elekitirodu, surfacing alurinmorin elekitirodu, nickel & cobalt alloy alurinmorin elekitirodu, ìwọnba irin & kekere alloy alurinmorin onirin, irin alagbara, irin alurinmorin onirin, gaasi-idabobo flux cored wires, aluminiomu alurinmorin onirin, submerged arc alurinmorin .wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 