E6010 erogba irin welding elekitirodu

Àpèjúwe Kúkúrú:

E6010 jẹ́ elekitirodu iru sodium rutile-cellulosic kan.


Àlàyé Ọjà

Àwọn àmì ọjà

AWS E6010 Electrode Alurinmorin Irin Onírẹlẹ̀

ÀWỌN ÌBÉÈRÈ:

O dara fun alurinmorin ti eto irin erogba kekere bi opo gigun, ikole ọkọ oju omi ati afara ati bẹbẹ lọ.

ÀWỌN ÌṢẸ̀LẸ̀:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

ÀWỌN ÌWÀN:

E6010 jẹ́ elekitirodu iru sodium rutile-cellulosic. A le so o pọ fun ipo gbogbo (paapaa fun ipo inaro-isalẹ) pẹlu DC+ nikan. O ni iṣẹ alurinmorin to dara julọ gẹgẹbi arc iduroṣinṣin, splatter kekere, yiyọ slag ti o rọrun ati agbara reintition ati bẹbẹ lọ. Iṣakoso adagun ti o ni didan ti o dara julọ, agbara arc ti o lagbara ati titẹ jinle ni ipo inaro-isalẹ.

ÌṢẸ̀DÁ KẸ́MÍKÀ TI GBOGBO ÌRÀN ÌLÚ: (ÌWỌ̀N %)

Àwọn ohun kan C Mn Si S P Ni Cr Mo V
Awọn ibeere ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Àwọn Àbájáde Àṣàrò 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

Àwọn OHUN ÈLÒ ÌṢẸ́-Ẹ̀RỌ̀ TI GBOGBO ÌRÀNLẸ̀ ALÁṢẸ́:

Àwọn ohun kan Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Awọn ibeere ≥430 ≥330 ≥20 ≥27
Àwọn Àbájáde Àṣàrò 475 400 26 80

Àkíyèsí:

1. Ni gbogbogbo, ko nilo lati tun gbẹ elekitiroodu naa ki o to so pọ. Ti o ba ni ọriniinitutu, o yẹ ki o tun gbẹ ẹ ni 70℃-90℃ fun wakati kan.

2. A gbọ́dọ̀ yọ ipata, epo, omi àti àwọn ẹ̀gbin mìíràn tí ó wà ní agbègbè ìsopọ̀ náà kúrò kí a tó fi ìsopọ̀ náà sí ara wọn.

ÀWỌN ÌLÀNÀ ÌṢẸ́ ÀWỌN OHUN TÓ WÀ NÍPA: (DC+)

Ìwọ̀n ìlà opin (mm) 2.5 3.2 4.0 5.0
Gígùn (mm) 300 350 400 400
Lọ́wọ́lọ́wọ́ (A) 50-80 60-100 100-140 140-180

ÀPÒ:

5kg/àpótí, àpótí 4/páálí, 20kgs/páálí, 50 káálí/páálí. 21MT -26MT fún 1X20″ FCL.

 

OEM/ODM:

A ṣe atilẹyin OEM/ODM ati pe a le ṣe apoti ni ibamu si apẹrẹ rẹ, jọwọ kan si wa fun ijiroro alaye.

 

Àwọn Ànímọ́ Lórí Lílò:

Apá tó dúró ṣinṣin gan-an.

O tayọ yiyọ ti slag.

Ìwọ̀lélẹ̀ kò jinlẹ̀.

Ooru ati ipata to dara.

O tayọ resistance kiraki.


  • Ti tẹlẹ:
  • Itele: