RBCuZn-B (Nickel Bronze) Brazing Filler Metals Welding Waya

Apejuwe kukuru:

RBCuZn-B Nickel Bronze (RBCuZn-B) irin kikun brazing jẹ iru si bronze ọgagun ṣugbọn o ni manganese ati irin eyiti o mu lile ati agbara ti idogo weld pọ si.


Alaye ọja

ọja Tags

RBCuZn-B Nickel Bronze (RBCuZn-B) irin kikun brazing jẹ iru si bronze ọgagun ṣugbọn o ni manganese ati irin eyiti o mu lile ati agbara ti idogo weld pọ si.O tun ni nickel ti o ni idaniloju pinpin iṣọkan ti irin ninu ohun idogo naa.Ina didoju tabi die-die oxidizing ati ṣiṣan boric acid/boric yẹ ki o lo.

AWS Kilasi: RBCuZn-B Iwe eri: AWS A5.8/A5.8M:2011
Alloy: RBCuZn-B ASME SFA A5.8

 

Ipo brazing: H, V Ibiti Brazing:
1620-1800F

 

Agbara Fifẹ, kpsi: 60-78
Ilọsiwaju%, min: 25

 

Ojuami Iyo 1620F Isokan 1590F Brinell Lile 80-110

Kemistri Waya Aṣoju bi fun AWS A5.8 (awọn iye ẹyọkan ni o pọju)

Cu Zn Sn Fe Mn Ni Pb Al Si Omiiran
56.0-60.0 Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0.50

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣe alabapin ninu iṣelọpọ awọn amọna alurinmorin, awọn ọpa alurinmorin, ati awọn ohun elo alurinmorin fun diẹ sii ju ọdun 20 lọ.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 

 