Alurinmorin Electrode AWS A5.4 E310Mo-16 Irin Alagbara Irin Alurinmorin Rods Stick Electrodes

Apejuwe kukuru:

A412 (AWS E310Mo-16) jẹ Cr26Ni21Mo2 funfun austenitic alagbara, irin elekiturodu pẹlu titanium kalisiomu ti a bo.


Alaye ọja

ọja Tags

Irin AlurinmorinElectrode

A412                                 

GB/T E310Mo-16

Aws A5.4 E310Mo-16

Apejuwe: A412 jẹ Cr26Ni21Mo2 mimọ austenitic alagbara, irin elekiturodu pẹlu titanium kalisiomu ti a bo.O le ṣee lo fun awọn mejeeji AC ati DC pẹlu iṣẹ ṣiṣe to dara julọ.Nitoripe molybdenum ti wa ni afikun si irin ti a fi silẹ, resistance pitting rẹ, agbara ooru ati idena kiraki ni gbogbo dara si ni akawe pẹlu A402 ati A407.

Ohun elo: O ti wa ni lilo fun alurinmorin ooru-sooro irin alagbara, irin ṣiṣẹ labẹ ga otutu ipo, ati ki o tun le ṣee lo fun alurinmorin alagbara, irin lining, dissimilar steels, bbl O ni o ni dara kiraki resistance nigbati alurinmorin erogba, irin ati kekere alloy, irin pẹlu ga hardenability. .

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.030

 

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Ilọsiwaju

%

Ẹri

≥550

≥25

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.0

2.5

3.2

4.0

5.0

Alurinmorin Lọwọlọwọ

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Akiyesi:

  1. Elekiturodu gbọdọ wa ni ndin fun wakati kan ni ayika 150 ℃ ṣaaju iṣẹ alurinmorin;
  2. Nitoripe ijinle ilaluja jẹ aijinile lakoko alurinmorin AC, ipese agbara DC yẹ ki o lo bi o ti ṣee ṣe lati ni ilaluja jinle.ati lọwọlọwọ ko yẹ ki o tobi ju lati yago fun pupa ti ọpa alurinmorin.

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣiṣẹ ni iṣelọpọ ti iṣelọpọ.alurinmorin elekiturodus, alurinmorin ọpá, atialurinmorin consumablesfun diẹ ẹ sii ju 20 ọdun.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 