AWS A5.23: ECNi1 Submerged Arc Welding Waya

Apejuwe kukuru:

AWS A5.23: ECNi1 jẹ elekiturodu okun waya ti o wa ni irin-kekere alloy fun alurinmorin arc submerged ni awọn ohun elo agbara giga.


Alaye ọja

ọja Tags

AWS A5.23: ECNi1 Submerged Arc Cored Wires Kekere Alloy Irin

Apejuwe

AWS A5.23: ECNi1 jẹ elekiturodu okun waya ti o wa ni irin-kekere alloy fun alurinmorin arc submerged ni awọn ohun elo agbara giga.o pade AWS A5.23 kemistri Ni1, ati pe o jẹ apẹrẹ fun awọn ipele agbara fifẹ loke 70 ksi.

Ohun elo akọkọ

Alurinmorin ẹyọkan ati ọpọ-ọpọlọpọ nipa lilo ṣiṣan ti a ṣe iṣeduro, ti kii ṣe alloyed ati awọn irin ọkà ti o dara, awọn irin oju ojo (laisi awọn ibeere ibaramu awọ), awọn iwọn otutu iṣẹ kekere, awọn tanki ibi ipamọ, awọn paati igbekalẹ, awọn panẹli ọkọ oju omi

● Iṣeto ati iṣelọpọ afara

●Iṣẹlẹ ti ita

● Awọn ohun elo ti o wuwo

● Ṣiṣe ọkọ oju omi

● Awọn tanki ipamọ

LOSIYI

Taara Electrode Rere lọwọlọwọ (DCEP), Taara Electrode Negetifu lọwọlọwọ (DCEN), Yiyi lọwọlọwọ (AC)

Standard diameters

1/8"(3.2 mm), 5/32"(4.0 mm)

Ìpamọ́

Ọja yẹ ki o wa ni ipamọ ni agbegbe gbigbẹ, ti paade, ati ninu apoti atilẹba rẹ ti ko tọ

Aws awọn iyasọtọ

 

 

 

 

AṢẸṢẸ KẸMIKÌKÌ IFỌ̀GBỌ́ WELD AGBÁRA*

 

 

ONÍṢẸ́ Ẹ̀RÁ AGBÁRA*

 

 

Awọn iye IPA TI APAPO CHAPY V-NOTS*

 

 

PARAMETERS NṢẸ AGBẸ́LẸ̀*

 

 

Mimu ilana alurinmorin to dara - pẹlu ooru ṣaaju ati awọn iwọn otutu interpass - le jẹ pataki ti o da
lori iru ati sisanra ti irin ni welded.
Awọn paramita ti pese fun awọn idi alaye nikan.Gbogbo iye wa ni isunmọ.Foliteji ti o dara julọ le yatọ (ni deede
± 2 volts) da lori yiyan ṣiṣan, sisanra ohun elo, apẹrẹ apapọ, ati awọn oniyipada miiran pato si ohun elo naa.
Bakanna, oṣuwọn ifisilẹ gangan le yatọ da lori yiyan ṣiṣan ati imọran olubasọrọ si ijinna iṣẹ.

 

 