H10MnSi AWS EM13K Submerged Arc Welding Waya

Apejuwe kukuru:

H10MnSi Submerged arc alurinmorin waya jẹ iru kan ti alabọde-manganese ati alabọde-alabọde iru alurinmorin waya.


Alaye ọja

ọja Tags

H10MnSi AWS EM13K Submerged Arc Welding Waya

EM13K 2.5/3.2/4.0/5.0mm Waya Alurinmorin Arc Submerged

H10MnSi Submerged arc alurinmorin waya jẹ iru kan ti alabọde-manganese ati alabọde-alabọde iru alurinmorin waya.
1. O baramu pẹlu alabọde-manganese ati alabọde-ohun alumọni iru alurinmorin ṣiṣan.
2. Ko ṣe akiyesi ipata lori irin ipilẹ.
3. O ni o ni o tayọ ileke igbáti ati slag detachability.
4. Monopole tabi dipole.AC/DC.
5. O ti wa ni lilo fun awọn mejeeji ga iyara alurinmorin ati ki o kikun alurinmorin lori 50kg kilasi mimọ awọn irin.
6. alurinmorin ti miiran 501 Mpa ipele erogba, irin ati kekere alloy, irin

EM13K Ṣe ibamu si Standard: GB/T 5293 H10MnSi
Aws EM13K
ISO 14171-B-SU25

Sipesifikesonu: O jẹ iru okun waya alurinmorin pẹlu manganese ti o yẹ ati akoonu ohun alumọni., O baamu pẹlu manganese kekere ati ṣiṣan iru alurinmorin-kekere, Aibikita si ipata lori irin ipilẹ.O ni idọti ileke ti o dara julọ, agbara iyọkuro slag ti o dara julọ.

Idi: Lilo pẹlu ṣiṣan sintered LT.SJ101, o le lo mejeeji fun iyara alurinmorin irin awo ti agbara fifẹ 420N / mm2 ati kikun alurinmorin.O ti wa ni lilo pupọ fun igbomikana alurinmorin, ọkọ oju omi titẹ, afara, ọkọ oju omi ati bẹbẹ lọ.

Iṣọkan Kemikali(%)

 

 

Kemikali Tiwqn C Mn Si S P Cr Ni Cu
Iye idaniloju ≤0.14 0.80 ~
1.10
0.60 ~
0.90
≤0.035 ≤0.035 ≤0.20 ≤0.30 ≤0.35
Abajade gbogbogbo 0.089 0.98 0.67 0.023 0.032 0.015 0.034 0.11

 
Mechanical Properties ti ohun idogo Irin

Ohun elo idanwo

Flux

Rm(MPa) ReL/Rp0.2(MPa) A(%) KV2(J)
-20℃
LT•SJ101 415-550 ≥330 ≥22 ≥27

 
Iwọn ti Welding Wires

Iwọn (mm) Φ2.5 Φ3.2 Φ4.0 Φ5.0

 