AWS E309L-15 Irin Alagbara Irin Alurinmo Awọn ọpa, Irin alagbara, irin solder Arc Welding Electrode

Apejuwe kukuru:

A067 (AWS E309L-15) jẹ kekere-hydrogen soda iru olekenka-kekere erogba Cr23Ni13 alagbara, irin elekiturodu.


Alaye ọja

ọja Tags

Irin AlurinmorinElectrode

A067                                         

GB/T E309L-15

Aws E309L-15

Apejuwe: A067 jẹ kekere-hydrogen soda iru olekenka-kekere erogba Cr23Ni13 alagbara, irin elekiturodu.Lo DCEP (taara ti isiyi elekiturodu rere) ati ki o le welded ni gbogbo awọn ipo.O ni akoonu erogba kekere, nitorinaa o le koju ibajẹ intergranular ti o ṣẹlẹ nipasẹ ojoriro carbide laisi awọn amuduro bii niobium ati titanium.

Ohun elo: O ti wa ni lilo fun awọn iru kanna ti irin alagbara, irin be, apapo irin ati ki o pataki-sókè irin irinše ni awọn iṣelọpọ ti sintetiki okun, petrochemical ati awọn miiran itanna.O tun le ṣee lo fun surfacing ti orilede fẹlẹfẹlẹ lori awọn akojọpọ odi ti iparun riakito titẹ ohun èlò ati alurinmorin ti ile-iṣọ ti abẹnu irinše.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Ilọsiwaju

%

Ẹri

≥520

≥25

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.5

3.2

4.0

5.0

Alurinmorin Lọwọlọwọ

(A)

50 ~ 70

80 ~ 120

130 ~ 160

160 ~ 200

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni ayika 300 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O ṣe pataki lati nu ipata, iwọn epo, omi, ati awọn impurities lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣiṣẹ ni iṣelọpọ ti iṣelọpọ.alurinmorin elekiturodus, alurinmorin ọpá, atialurinmorin consumablesfun diẹ ẹ sii ju 20 ọdun.

Awọn ọja akọkọ wa pẹlu irin alagbaraalurinmorin elekiturodus, erogba irin alurinmorin elekitirodu, kekere alloy alurinmorin elekitirodu, surfacing alurinmorin elekitirodu, nickel & cobalt alloy alurinmorin elekitirodu, ìwọnba irin & kekere alloy alurinmorin onirin, irin alagbara, irin alurinmorin onirin, gaasi-idabobo flux cored wires, aluminiomu alurinmorin onirin, submerged arc alurinmorin .wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.