Awọn elekitirodi Welding Hardfacing DIN 8555 (E1-UM-350) Awọn ọpa Alurinmorin dada, Wọ Electrode Stick Resistant

Apejuwe kukuru:

DIN 8555 (E1-UM-350) jẹ elekiturodu SMAW ti o ni ipilẹ ti a bo fun kiraki ati yiya dada sooro.


Alaye ọja

ọja Tags

Hardfacing WeldingElectrode

 

Standard: DIN 8555 (E1-UM-350)

Iru No.: TY-C DUR 350

 

Sipesifikesonu & Ohun elo:

· Ipilẹ ti a bo SMAW elekiturodu fun kiraki ati ki o wọ sooro surfacing.

· Ti o dara abrasion resistance.Rọrun lati weld ni gbogbo awọn ipo.

Paapa ti baamu fun yiya sooro surfacing on Mn-Cr-V alloyed awọn ẹya ara, gẹgẹ bi awọn ọpọlọ, orin rollers, pq support yipo, sprocket wili, itọsọna yipo ati be be lo.

 

Apapọ kemikali ti irin ti a fi silẹ (%):

 

C

Si

Mn

Cr

Fe

DIN

-

-

-

-

-

EN

-

-

-

-

-

Aṣoju

0.20

1.2

1.40

1.8

Bal.

 

 

Lile irin ti a fi silẹ:

Bi Welded

(HB)

1 Layer lori irin pẹlu C = 0.5%

(HB)

370

420

 

Awọn abuda gbogbogbo:

· Microstructure Ferrite + Martensitic

· Machinability O dara pẹlu Tungsten carbides tipped irinṣẹ

· Preheating Preheat awọn ẹya eru ati awọn irin fifẹ giga si 250-350 ℃

· Tun ṣe atunṣe fun awọn wakati 2 ni 300 ℃ ṣaaju lilo.

 