E308L-17 Irin Alurinmorin Rod

Apejuwe kukuru:

E308L-17 Fun Irin Alagbara Irin Welding Electrode Opa Alurinmorin (Kekere C, 18%Cr- 8%Ni)


Alaye ọja

ọja Tags

E308L-17 Fun Irin Alagbara Irin Welding Electrode Opa Alurinmorin (Kekere C, 18%Cr- 8%Ni)

Awọn ipin

EN IS03581-A:2016: E 19 9 L R 12

EN IS03581-B: 2016: ES308L-17

Aws A5.4-2014: E308L-17

JISZ 3221-2013: ES308L-17

Apejuwe

Ibora jẹ iru titania orombo wewe fun alurinmorin ti 18% Cr-8% Ni irin alagbara, irin.(AISI 301, 302, 304, 308)

-Ailewu alurinmorin ti o dara julọ nitori oṣuwọn fifisilẹ giga.

-Yọ Omi, ipata, epo ati gbogbo awọn ajeji ọrọ lati yara saju si alurinmorin.

-Ti o dara lilo pẹlu taara lọwọlọwọ ohun elo.

-Preheating jẹ ko wulo ni apapọ.

Tun elekiturodu tun ni 250 ~ 350 ° C fun awọn iṣẹju 30 ~ 60 ṣaaju lilo.

Irin Idogo Kemikali (%)
C Mn Si Cr Ni S P Mo Cu Fn
0.03 0.65 0.73 18.95 9.82 0.012 0.028 0.21 0.30 6.4

 

Awọn iwọn & Niyanju Lọwọlọwọ (AC tabi DC)
Alurinmorin opa opin
(mm)
2.5 3.2 4.0 5.0
alurinmorin lọwọlọwọ
(A)
55-80 90-130 110-150 140-180

Awọn abuda lori Lilo:

Aaki iduroṣinṣin pupọ.

O tayọ yiyọ ti slag.

Ilaluja jẹ aijinile.

Ti o dara ooru ati ipata resistance.

O tayọ kiraki resistance.

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣe alabapin ninu iṣelọpọ awọn amọna alurinmorin, awọn ọpa alurinmorin, ati awọn ohun elo alurinmorin fun ọdun 22.

Awọn ọja akọkọ wa pẹlu awọn ohun elo irin alagbara irin alagbara, awọn amọna alurinmorin erogba, awọn elekitirodi alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy welding electrodes, ìwọnba irin & kekere alloy alurinmorin onirin, irin alagbara, irin alurinmorin onirin, gaasi shielded flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.onirin, nickel & cobalt alloy alurinmorin onirin, idẹ alurinmorin onirin, TIG & MIG alurinmorin onirin, tungsten amọna, erogba gouging amọna ati awọn miiran alurinmorin awọn ẹya ẹrọ & consumables.