Low Alloy Irin Welding Electrode Aws E9016-D1

Apejuwe kukuru:

J606 (AWS E9016-D1) jẹ elekiturodu irin-giga-kekere alloy ti o ni iwọn kekere-hydrogen potasiomu ti a bo.O le ṣee lo fun gbogbo-ipo alurinmorin pẹlu AC ati DC.Iduroṣinṣin iṣẹ ti alurinmorin AC kere si ti alurinmorin DC.


Alaye ọja

ọja Tags

Low Alloy Irin Welding Electrode

J606                                       

GB/T E6016-D1

Aws E9016-D1 

 

Apejuwe: J606 jẹ elekiturodu irin-giga ti o ni agbara-kekere ti o ni iwọn kekere-hydrogen potasiomu ti a bo.O le ṣee lo fun gbogbo-ipo alurinmorin pẹlu AC ati DC.Iduroṣinṣin iṣẹ ti alurinmorin AC kere si ti alurinmorin DC. 

Ohun elo: Lo fun alurinmorin alabọde erogba irin ati kekere-alloy ga-agbara irin awọn ẹya ti o baamu agbara, gẹgẹ bi awọn Q420, ati be be lo.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1,75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Iye ipa (J)

-30 ℃

Ẹri

≥590

≥490

≥15

≥27

Idanwo

620 ~ 680

≥500

20 ~ 28

≥27

 

Akoonu hydrogen tan kaakiri ti irin ti a fi silẹ: ≤4.0mL/100g (ọna glycerin)

Ayewo X-ray: Mo ite

 

Iṣeduro lọwọlọwọ:

(mm)

Opa opin

2.0

2.5

3.2

4.0

5.0

5.8

(A)

Alurinmorin Lọwọlọwọ

40 ~ 70

70 ~ 90

90 ~ 120

140 ~ 180

180 ~ 220

210 ~ 260

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni 350 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O jẹ pataki lati nu soke ipata, epo asekale, omi, ati impurities lori alurinmorin awọn ẹya ara ṣaaju ki o to alurinmorin;

3. Lo kukuru arc isẹ nigba alurinmorin.Awọn orin alurinmorin dín to dara;

4. Nigbati apakan weld ba nipọn, o yẹ ki o wa ni preheated si loke 150 ° C ati ki o tutu laiyara lẹhin alurinmorin.

 




  • Ti tẹlẹ:
  • Itele: