Ọpá alurinmorin AWS A5.11 ENiCrFe-3 nickel orisun Alloy Welding Electrodes, nickel Arc Welding Rods

Apejuwe kukuru:

Ni307-3 (AWS ENiCrFe-3) jẹ elekiturodu ti o da lori nickel pẹlu iṣu iṣu soda hydrogen-kekere.Lo DCEP (daadaa elekiturodu lọwọlọwọ taara).


Alaye ọja

ọja Tags

Nickel ati Nickel Alloy Welding Electrode

Ni307-3                                                     

GB/T ENi6182

Aws A5.11 ENiCrFe-3

Apejuwe: Ni307-3 ni anickel-orisun elekiturodu pẹlu kekere-hydrogen soda ti a bo.Lo DCEP (daadaa elekiturodu lọwọlọwọ taara).O ni o ni ti o dara kiraki resistance nitori awọn weld ni kan awọn iye ti manganese, niobium, ati awọn miiran alloying eroja.

Ohun elo: O ti wa ni lilo fun awọn alurinmorin tinickel-chromium-iron alloys (gẹgẹ bi awọn UNS N06600) ati awọn surfacing ti irin.Iwọn otutu ti n ṣiṣẹ ni gbogbogbo ko ga ju 480 ° C, ati pe resistance kiraki dara.Dara fun ohun elo titẹ ileru atomiki ati alurinmorin ojò kemikali.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Fe

P

S

Si

Cu

≤0.10

5.0 ~ 10.0

≤10.0

≤0.020

≤0.015

≤1.0

≤0.5

Ni

Ti

Mo

Nb

Ta

Omiiran

 

≥60.0

≤1.0

13.0 ~ 17.0

1.0 ~ 3.5

≤0.30

≤0.50

 

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Ẹri

≥550

≥360

≥27

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.5

3.2

4.0

5.0

Alurinmorin lọwọlọwọ

(A)

60 ~ 90

80 ~ 100

110 ~ 150

130 ~ 180

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun1 wakati ni ayika 300 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O ṣe pataki lati nu ipata, epo, omi, ati awọn idoti lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.Gbiyanju lati lo aaki kukuru lati weld.

 


  • Ti tẹlẹ: