Apejuwe kukuru:

Ni327 -6 (AWS A5.11 ENiCrMo-6) jẹ elekiturodu ti o da lori nickel pẹlu iṣuu soda soda kekere-hydrogen.Lo DCEP (daadaa elekiturodu lọwọlọwọ taara).


Alaye ọja

ọja Tags

Nickel ati Nickel Alloy Welding Electrode

Ni327-6                                                     

GB/T ENi6620

Aws A5.11 ENiCrMo-6

Apejuwe: Ni327 -6 jẹ elekiturodu ti o da lori nickel pẹlu ideri iṣuu soda kekere-hydrogen.Lo DCEP (elekiturodu lọwọlọwọ taararere).Awọn ohun idogo irin ni o ni o tayọ plasticity, toughness ati kiraki resistance.Irin ti a fi pamọ ni olùsọdipúpọ imugboroja laini ti o jọra si ti irin, ati pe o ni agbara giga ati ipata ipata ni iwọn otutu yara ati iwọn otutu giga.

Ohun elo: O ti wa ni lilo fun awọn alurinmorin ti Ni9% irin, ati ki o le tun ti wa ni lo fun alurinmorin ti dissimilar steels ati soro-to-weld alloys.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Ni

Mo

Fe

Cu

≤0.10

2.0 ~ 4.0

≤1.0

≥55.0

5.0 ~ 9.0

≤10.0

≤0.5

Nb + Ta

W

Cr

S

P

Omiiran

 

0.5 ~ 2.0

1.0 ~ 2.0

12.0 ~ 17.0

≤0.015

≤0.020

≤0.5

 

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Ẹri

≥620

≥350

≥32

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.5

3.2

4.0

Alurinmorin lọwọlọwọ

(A)

50 ~ 70

80 ~ 100

110 ~ 150

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun1 wakati ni ayika 300 ℃ ṣaaju ki o to alurinmorin isẹ ti.Gbiyanju lati lo arc kukuru lati weld;

2. O ṣe pataki lati nu ipata, epo, omi, ati awọn idoti lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.

3. Gbiyanju lati lo kekere agbara ila nigba alurinmorin, olona-Layer ati olona-kọja alurinmorin.

 

 