Didara Didara Ti o dara julọ Tyue Brand AWS A5.11 ENiCu-7 Awọn elekitirodi ti o da lori Nickel, Awọn ọpa alurinmorin Nickel Alloy fun Arc Welding

Apejuwe kukuru:


Alaye ọja

ọja Tags

Nickel ati Nickel Alloy Welding Electrode

Ni207                                                     

GB/T ENi4060

Aws A5.11 ENiCu-7

Apejuwe: Ni207 jẹ elekiturodu alloy Monel pẹlu iṣuu soda hydrogen kekere.Lo DCEP (taara ti isiyi elekiturodu rere) ati ki o ni ti o dara alurinmorin išẹ ati kiraki resistance.

Ohun elo: Fun alurinmorin Monel tabi awọn irin ti o yatọ.O tun le ṣee lo fun apọju alurinmorin orilede Layer.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Fe

Si

Al

Ti

Cu

Nb

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤1.0

≤1.0

27.0 ~ 34.0

≤2.5

≥62.0

≤0.015

≤0.020

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Ẹri

≥480

≥200

≥27

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

3.2

4.0

Alurinmorin lọwọlọwọ

(A)

90 ~ 110

110 ~ 150

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 2 wakati ni ayika 300 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O ṣe pataki lati nu ipata, epo, omi, ati awọn idoti lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.Gbiyanju lati lo aaki kukuru lati weld.

 