Tyue Brand AWS ENiCrMo-4 Nickel ati Nickel orisun Alloy Welding Electrode, Awọn ọpa Alurinmorin Arc ti o dara julọ, Olupese Welding

Apejuwe kukuru:

Ni327-4 (ENiCrMo-4) jẹ elekiturodu ti o da lori nickel pẹlu iṣuu iṣuu soda kekere-hydrogen.Lo DCEP (daadaa elekiturodu lọwọlọwọ taara).


Alaye ọja

ọja Tags

Nickel ati Nickel Alloy Welding Electrode

Ni327-4                                                     

GB/T ENi6276

Aws A5.11 ENiCrMo-4

 

Apejuwe: Ni327-4 jẹ elekiturodu ti o da lori nickel pẹlu ideri iṣuu soda kekere-hydrogen.Lo DCEP (elekiturodu lọwọlọwọ taararere).O ni iṣẹ alurinmorin ti o dara julọ pẹlu ijona aaki iduroṣinṣin, spatter ti o dinku, yiyọ slag rọrun,

ati ki o lẹwa weld.Awọn ohun-ini ẹrọ ti irin ti a fi silẹ jẹ iduroṣinṣin.

 

Ohun elo: Lo fun alurinmorin kekere-carbon nickel-chromium-molybdenum alloys, gẹgẹ bi awọn Hastelloy C276, ASTM B574, B575, B619, B622, B626, ati ki o le tun ti wa ni lo fun alurinmorin dissimilar steels pẹlu miiran nickel-orisun alloys.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Cr

Ni

Mo

≤0.02

≤1.0

≤0.2

14.5 ~ 16.5

≥50.0

15.0 ~ 17.0

W

Co

Fe

S

P

Omiiran

3.0 ~ 4.5

≤2.5

4.0 ~ 7.0

≤0.015

≤0.020

≤0.5

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Ẹri

≥690

≥400

≥22

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.5

3.2

4.0

Alurinmorin lọwọlọwọ

(A)

60 ~ 90

70 ~ 110

90 ~ 150

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun1 wakati ni ayika 300 ℃ ṣaaju ki o to alurinmorin isẹ ti.Gbiyanju lati lo arc kukuru lati weld;

2. O ṣe pataki lati nu ipata, epo, omi, ati awọn idoti lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.

3. Gbiyanju lati lo kekere agbara ila nigba alurinmorin, olona-Layer ati olona-kọja alurinmorin.

 