Àwọn amúlétutù ENiCrFe-3 fún Nickel

Àpèjúwe Kúkúrú:

Ẹ̀rọ itanna ń gbé irin 65Ni-20Cr-2Nb-1.5Mo tí a fi weld ṣe jáde.


Àlàyé Ọjà

Àwọn àmì ọjà

Kóòdù ISO EN: 14172:ENi6082

Electrode n fi irin weld 65Ni-20Cr-2Nb-1.5Mo silẹ. Irin weld didara redio ti o ni awọn agbara to ga julọ. O dara julọ fun awọn alloy welding ti awọn akopọ kanna si ara wọn, fun oju irin pẹlu alloy Nickel-Chromium-Iron nigbati akoonu Manganese giga ko ba ni ipalara, fun wiwọ ti a fi aṣọ welding ti irin ti a fi aṣọ welding ti Nickel Chromium-Iron ati awọn akojọpọ irin ti o yatọ si ara wọn. O dara fun ibora ti awọn awo forge. A ṣeduro pataki fun wiwọ 9% Ni Steels fun iṣẹ cryogenic. A tun lo fun wiwọ ti awọn alloy Nickel-Chromium ti a lo fun awọn ohun elo otutu giga bi awọn eroja igbona ileru ati awọn tubes atunṣe.

ÌṢẸ̀DÁ KẸ́MÍKÍRÌ ÀWỌN IRÁNṢẸ́ TÓ WÀ NÍPASẸ̀

Ohun èlò C Mn Si Cr Ni Fe Nb Cu Ti S P
Ogorun ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

Àwọn OHUN ÈLÒ ÌṢẸ́-Ẹ̀KỌ̀ ÀWỌN OHUN ÈLÒ TÓ WÀ NÍNÚ GBOGBO ÌRÀN WÍLẸ̀

UTS YS Gbigbọn Agbára Ìpa CVN (J) Ìfẹ̀sí ẹ̀gbẹ́ Agbara Ríròrò ní
(MPa) (MPa) (L= 5d)% ní Dínkù 196°C ní ìyọkúrò 196°C (mm) 600°C fún wákàtí 1000.
620 500 30 75 0.85 160 MPa

DÁTÍ TÓ WÀ NÍṢẸ́KÌ ÀTI TÓ WÀ NÍPAKÌ: DC (+)

Ìwọ̀n (mm)

Díà x Gígùn

5×350

4×350

3.15×350

2.5×350

Ipele lọwọlọwọ (Amps)

150-180

120-150

80-110

60-70

Ìwúwo/Páálítì (kgs)

2.5

2.5

2.5

2.5

Ìṣọ́ra

1. Rí i dájú pé àwọn elekitiroodu náà gbẹ. Tún gbẹ àwọn elekitiroodu náà ní 300-325°C fún wákàtí kan.

2. Máa lo ìró gígùn, kí o sì dín ooru tí ó wà nínú rẹ̀ kù.

3. Jẹ́ kí ìsopọ̀ náà tutù sí ìsàlẹ̀ 50 C kí ó tó di pé ó gbóná, èyí tó tẹ̀lé e.