AWS A5.4 E316L-16 Irin Alagbara Irin Alurinmorin Awọn ọpa Olupese Awọn ohun elo Alurinmorin to dara julọ

Apejuwe kukuru:

A022 (AWS A5.4 E316L-16) jẹ erogba-kekere carbon Cr18Ni12Mo2 alagbara, irin elekiturodu pẹlu titanium kalisiomu ti a bo.


Alaye ọja

ọja Tags

Irin Alagbara, Irin Welding Electrode

A022                                                 

GB/T E316L-16

Aws E316L-16

Apejuwe: A022 jẹ erogba-kekere carbon Cr18Ni12Mo2 alagbara, irin elekiturodu pẹlu titanium kalisiomu ti a bo.O le ṣee lo fun awọn mejeeji AC ati DC pẹlu ti o dara ilana iṣẹ.Akoonu erogba ti irin ti a fi silẹ jẹ ≤0.04%, eyiti o pese pẹlu itọju ooru ti o dara, ipata ipata ati idena kiraki.

 Ohun elo: O ti wa ni lilo fun alurinmorin urea, sintetiki okun ati awọn miiran itanna ati awọn kanna iru ti irin alagbara, irin be.O tun le ṣee lo fun irin alagbara chromium, irin apapo ati irin ti o yatọ ti ko le ṣe itọju ooru lẹhin alurinmorin.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Ilọsiwaju

%

Ẹri

≥490

≥30

 

Iṣeduro lọwọlọwọ:

Opa opin

(mm)

2.0

2.5

3.2

4.0

5.0

Alurinmorin Lọwọlọwọ

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni ayika 150 ℃ ṣaaju ki o to alurinmorin isẹ;

2. Nitori awọn ilaluja ijinle ni aijinile nigba AC alurinmorin, awọn DC ipese agbara yẹ ki o ṣee lo bi Elo bi o ti ṣee lati gba jinle ilaluja.ati lọwọlọwọ ko yẹ ki o tobi ju lati yago fun pupa ti ọpa alurinmorin;

3.The ipata resistance ti irin ti a fi silẹ ni ipinnu nipasẹ adehun meji ti ipese ati eletan.

 

Wenzhou Tianyu Itanna Co., Ltd ti dasilẹ ni ọdun 2000. A ti ṣe alabapin ninu iṣelọpọ awọn amọna alurinmorin, awọn ọpa alurinmorin, ati awọn ohun elo alurinmorin fun diẹ sii ju ọdun 20 lọ.

Awọn ọja akọkọ wa pẹlu awọn amọna alurinmorin irin alagbara, irin alagbara, awọn elekitirodi alurinmorin, awọn amọna alurinmorin kekere, awọn ẹrọ itanna alurinmorin, awọn amọna alurinmorin nickel & cobalt alloy, awọn onirin irin kekere & kekere alloy alurinmorin, awọn irin alagbara irin alurinmorin, irin alagbara, irin alurinmorin, gaasi-dabobo flux cored wires, aluminiomu alurinmorin onirin, submerged aaki alurinmorin.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 


  • Ti tẹlẹ:
  • Itele: