Ìsọ̀rí AWS: AWS 5.9
ÀPÈJÚWE:
Wáyà ìsopọ̀mọ́ra irin alagbara ní agbára ìbòrí gíga, iṣẹ́ ìmọ̀-ẹ̀rọ ìsopọ̀mọ́ra tó dára ní gbogbo ipò ìsopọ̀mọ́ra. Wọ́n wọ́pọ̀ ní ilé-iṣẹ́: ìṣètò ilé, ọkọ̀, ìmọ̀-ẹ̀rọ afárá, ẹ̀rọ iwakusa, ọkọ̀ ojú irin, páìpù epo, ẹ̀rọ tí ń gbé ìfúnpá gaasi, ẹ̀rọ agbára, àti bẹ́ẹ̀ bẹ́ẹ̀ lọ.
Nọ́mbà Àwòṣe àti Ìwọ̀n:
1. Ipese ile-iṣẹ iṣẹ OEM.
2. Àwòṣe: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi àti bẹ́ẹ̀ bẹ́ẹ̀ lọ.
3. Ìwọ̀n wáyà MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Ìwọ̀n wáyà TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
ÌFÍHÀN:
A n pese oniruuru waya irin alagbara, pẹlu okun waya Mig solid welding, okun waya Tig rod welding ati okun waya submerged-arc welding, gbogbo wọn ni didara giga ati pe a n ta wọn kaakiri agbaye.
Yàtọ̀ sí 308 àti 309, a tún ń fúnni ní 304, 321, 347, 316L, 310, 2209, àti 201. Bákan náà pẹ̀lú àwọn ìlànà pàtàkì bíi 318L, 904L, 2594, NiCrMo-3, Ni1.
ÀKÓJỌ:
Iṣakojọpọ waya alurinmorin Mig (spool ati drum pack)
Ìwọ̀n ...
Àpò: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/spool, 200 kg/spool
Iṣakojọpọ waya alumọni Tig rod (ọpọn ṣiṣu)
Ìwọ̀n ...
Àpò: 5 kg/àpò
Wáìlì ìrọ̀lẹ̀ aaki tí a rì sínú omi
Ìwọ̀n ...
Àpò: 20kg/àpò, 25 kg/àpò
A kaabo apoti didoju ati OEM!
ÀWỌN ÌṢẸ̀LẸ̀ KẸ́MÍKÀ TI WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ WÁYÀ:
| Nọmba awoṣe | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Nọmba awoṣe | Agbára ìfàsẹ́yìn Rm(Mpa) | Agbara ikore Rel tabi Rp0.2 (Mpa) | Gbigbọn (%) | Nọmba awoṣe | Agbára ìfàsẹ́yìn Rm(Mpa) | Agbara ikore Rel tabi Rp0.2 (Mpa) | Gbigbọn (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| Tiwqn waya irin alagbara TIG ati MIG ti a ṣe pẹlu irin alagbara TIG ati MIG | ||||||||||
| YB5092-2005 | AWS | Àkójọpọ̀ Kẹ́míkà % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | ER453s | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
Wọ́n dá Wenzhou Tianyu Electronic Co., Ltd sílẹ̀ ní ọdún 2000. A ti ń ṣe iṣẹ́ àwọn elekitirodu ìfọwọ́sowọ́pọ̀, ọ̀pá ìfọwọ́sowọ́pọ̀, àti àwọn ohun èlò ìfọwọ́sowọ́pọ̀ fún ohun tó lé ní ogún ọdún.
Àwọn ọjà pàtàkì wa ní àwọn elekitirodu ìsopọ̀ irin alagbara, àwọn elekitirodu ìsopọ̀ irin erogba, àwọn elekitirodu ìsopọ̀ irin aláwọ̀ dúdú, àwọn elekitirodu ìsopọ̀ ojú, àwọn elekitirodu ìsopọ̀ nickel & cobalt, àwọn waya ìsopọ̀ irin aláwọ̀ dúdú àti oníwọ̀n, àwọn waya ìsopọ̀ irin aláwọ̀ dúdú, àwọn waya ìsopọ̀ irin aláwọ̀ dúdú tí a fi gáàsì dáàbò bò, àwọn waya ìsopọ̀ aluminiomu, àwọn waya ìsopọ̀ arc tí a fi sínú omi, àwọn waya ìsopọ̀ nickel & cobalt, àwọn waya ìsopọ̀ idẹ, àwọn waya ìsopọ̀ TIG & MIG, àwọn elekitirodu tungsten, àwọn elekitirodu ìsopọ̀ erogba, àti àwọn ohun èlò ìsopọ̀ àti àwọn ohun èlò míràn tí a lè lò.