AWS E8018-C1 Irin Alurinmorin Electrode W606Fe Low Hydrogen ARC Awọn ọpa Alurinmorin

Apejuwe kukuru:

W606Fe (AWS E8018-C1) jẹ elekiturodu irin ni iwọn otutu kekere kan pẹlu lulú irin ati ideri potasiomu hydrogen kekere


Alaye ọja

ọja Tags

Iwọn otutu kekereIrin AlurinmorinElectrode

W606Fẹ                                                     

GB/T E5518-C1

Aws A5.5 E8018-C1

Apejuwe: W606Fe jẹ elekiturodu irin ni iwọn otutu kekere pẹlu lulú irin ati ideri potasiomu kekere kan ti hydrogen.O le ṣee lo fun gbogbo-ipo alurinmorin pẹlu AC ati DC.Irin ti a fi silẹ ni ipa lile to dara ni -60°C. 

Ohun elo: Lo fun alurinmorin kekere, irin bi 2.5Ni.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

≤0.80

2.00 ~ 2,75

≤0.020

≤0.025

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Iye ipa (J)

-60℃

Ẹri

≥540

≥440

≥17

≥27

 

Akoonu hydrogen tan kaakiri ti irin ti a fi silẹ: ≤6.0mL/100g (ọna glycerin) tabi ≤10mL/100g (Makiuri tabi ọna chromatography gaasi)

Ayewo X-ray: Mo ite

 

Iṣeduro lọwọlọwọ:

(mm)

Opa opin

3.2

4.0

5.0

(A)

Alurinmorin Lọwọlọwọ

90 ~ 120

140 ~ 180

180 ~ 210

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni 350 ℃ ṣaaju ki awọn alurinmorin isẹ;

2. O ṣe pataki lati nu ipata, iwọn epo, omi, ati awọn impurities lori awọn ẹya alurinmorin ṣaaju ṣiṣe alurinmorin.

 