W707 (AWS E7015-G) jẹ elekiturodu irin ti o ni iwọn otutu ti o ni iwọn-kekere ti iṣu soda iṣuu soda.


Alaye ọja

ọja Tags

Low otutu Irin Welding Electrode

W707                                                     

GB/T E5015-G

Aws A5.5 E7015-G

Apejuwe: W707 jẹ elekiturodu irin-iwọn otutu ti o ni iwọn-kekere ti iṣu soda iṣuu soda.Lo DCEP (taara ti isiyi elekiturodu rere) ati ki o le welded ni gbogbo awọn ipo.Irin ti a fi pamọ si tun ni ipa lile to dara ni -70°C.

Ohun elo: Lo fun alurinmorin kekere, irin bi 2.5Ni.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.25

≤0.60

2.00 ~ 2,75

≤0.020

≤0.025

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Iye ipa (J)

-70 ℃

Ẹri

≥490

≥390

≥22

≥27

 

Akoonu hydrogen tan kaakiri ti irin ti a fi silẹ: ≤6.0mL/100g (ọna glycerin) tabi ≤10mL/100g (Makiuri tabi ọna chromatography gaasi)

Ayewo X-ray: Mo ite

 

Iṣeduro lọwọlọwọ:

(mm)

Opa opin

2.0

2.5

3.2

4.0

5.0

(A)

Alurinmorin Lọwọlọwọ

40 ~ 70

70 ~ 100

90 ~ 120

140 ~ 180

170 ~ 210

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni 350 ℃ ṣaaju ki o to alurinmorin isẹ;

2. Gbiyanju lati lo kekere agbara ila nigba alurinmorin, olona-Layer ati olona-kọja alurinmorin.