AWS E7015-G Irin Alurinmorin Electrode W607 Low-Hydrogen Weld Rod

Apejuwe kukuru:

W607 (AWS E7015-G) jẹ elekiturodu irin ti o ni iwọn otutu ti o ni iwọn kekere ti iṣu soda iṣuu soda.


Alaye ọja

ọja Tags

Low otutu Irin Welding Electrode

W607                                                     

GB/T E5015-G

Aws A5.5 E7015-G

 

Apejuwe: W607 jẹ elekiturodu irin-iwọn otutu ti o ni iwọn kekere-hydrogen iṣuu soda.Lo DCEP (taara ti isiyi elekiturodu rere) ati ki o le welded ni gbogbo awọn ipo.Irin ti a fi silẹ ni ipa lile to dara ni -60°C.

Ohun elo: Ti a lo fun alurinmorin irin iwọn otutu kekere bii 09MnD.

 

Apapọ kemikali ti irin weld (%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.65

≤0.60

0.50 ~ 2.50

≤0.020

≤0.025

 

Awọn ohun-ini ẹrọ ti irin weld:

Ohun elo idanwo

Agbara fifẹ

Mpa

Agbara ikore

Mpa

Ilọsiwaju

%

Iye ipa (J)

-60℃

Ẹri

≥490

≥390

≥22

≥27

 

Akoonu hydrogen tan kaakiri ti irin ti a fi silẹ: ≤6.0mL/100g (ọna glycerin) tabi ≤10mL/100g (Makiuri tabi ọna chromatography gaasi)

Ayewo X-ray: Mo ite

 

Iṣeduro lọwọlọwọ:

(mm)

Opa opin

2.0

2.5

3.2

4.0

5.0

(A)

Alurinmorin Lọwọlọwọ

40 ~ 70

60 ~ 90

100 ~ 120

140 ~ 170

170 ~ 200

 

Akiyesi:

1. Awọn elekiturodu gbọdọ wa ni ndin fun 1 wakati ni 350 ℃ ṣaaju ki o to alurinmorin isẹ;

2. O jẹ pataki lati nu soke ipata, epo asekale, omi, ati impurities lori alurinmorin awọn ẹya ara ṣaaju ki o to alurinmorin;

3. Apakan ti a fi wewe le jẹ preheated ni iwọn 150 ° C ṣaaju alurinmorin lati dena awọn dojuijako.

 