AWS A5.18 ER70S-6 Erogba Irin Welding Wire Metals fun Gas Shield Arc Welding, Awọn onirin to lagbara

Apejuwe kukuru:

ER70S6 jẹ okun waya alurinmorin irin ìwọnba ti o ni awọn ipele ti o ga julọ ti manganese ati ohun alumọni ju awọn iwọn boṣewa miiran ti okun waya MIG si ọja awọn weld didara giga nigba lilo lori idọti, ororo, tabi irin ipata.


Alaye ọja

ọja Tags

ER70S6 jẹ okun waya alurinmorin irin ìwọnba ti o ni awọn ipele ti o ga julọ ti manganese ati ohun alumọni ju awọn iwọn boṣewa miiran ti okun waya MIG si ọja awọn weld didara giga nigba lilo lori idọti, ororo, tabi irin ipata.Akoonu ohun alumọni ti o ga julọ mu omi ṣiṣan ti adagun weld pọ si, nitorinaa ṣiṣẹda irisi ilẹkẹ didan ati abajade ni lilọ-lẹhin-weld pọọku.Okun waya yii jẹ iṣẹ-ṣiṣe lati pese laisi porosity, awọn alurin didara x-ray ni agbara fifẹ ti o ga julọ (gẹgẹbi welded) ti gbogbo awọn okun onirin erogba lasan.

Awọn ohun elo Aṣoju: awọn ohun elo itaja gbogboogbo pẹlu aiṣedeede ti ko dara tabi ipata, awọn awo epo;irin simẹnti tabi forging igbala;ile ise agbese;irin dì;awọn tanki;iṣẹ ikole

AWS Kilasi: ER70S6

Iwe eri: AWS A5.18/A5.18M:2005

Alloy: ER70S6

ASME SFA A5.18

Ipo alurinmorin: F, V, OH, H

Lọwọlọwọ: DCEP

Agbara Fifẹ, kpsi:

70

Agbara ikore, kpsi:

58

Ilọsiwaju ni 2"%:

22

Kemistri Waya Aṣoju gẹgẹbi fun AWS A5.18 (awọn iye ẹyọkan ni o pọju)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1.85

0.80-1.15

0.025

0.035

0.15

0.15

0.15

0.03

0.50

Aṣoju Welding Parameters

Iwọn opin

Ilana

Folti

Iyara Irin-ajo

Amps

Gaasi Idaabobo

in

(mm)

(ipm)

.035

(0.9)

GMAW

23-26

11-22

160-300

Sokiri Gbigbe 98% Argon + 2% Atẹgun

.045

(1.2)

GMAW

23-29

12-21

170-375

Sokiri Gbigbe 98% Argon + 2% Atẹgun

1/16

(1.6)

GMAW

25-31

9-19

275-475

Sokiri Gbigbe 98% Argon + 2% Atẹgun

.023

GMAW

14-19

10-15

30-85

Gbigbe Circuit Kukuru 98% Argon + 2% Atẹgun

.030

(0.8)

GMAW

15-20

12-24

40-130

Gbigbe Circuit Kukuru 98% Argon + 2% Atẹgun

.035

(0.9)

GMAW

16-25

11-40

60-235

Gbigbe Circuit Kukuru 98% Argon + 2% Atẹgun

.045

(1.14)

GMAW

18-23

12-22

90-290

Gbigbe Circuit Kukuru 98% Argon + 2% Atẹgun

.035

(0.9)

GTAW

12-15

N/A

60-100

100% Argon

.045

(1.14)

GTAW

13-16

N/A

70-120

100% Argon

1/16

(1.6)

GTAW

12

N/A

100-160

100% Argon

1/16- 3/32

(1.6)-(2.4)

GTAW

12

N/A

120-250

100% Argon

1/8

(3.2)

GTAW

12

N/A

150-300

100% Argon